High Temperature Flow Behavior of Ultra-Strong Nanoporous Au assessed by Spherical Nanoindentation
Research output: Contribution to journal › Article › Research › peer-review
Standard
High Temperature Flow Behavior of Ultra-Strong Nanoporous Au assessed by Spherical Nanoindentation. / Leitner, Alexander; Maier-Kiener, Verena; Kiener, Daniel.
In: Nanomaterials, Vol. 8.2018, No. 6, 366, 24.05.2018, p. 1-12.
In: Nanomaterials, Vol. 8.2018, No. 6, 366, 24.05.2018, p. 1-12.
Research output: Contribution to journal › Article › Research › peer-review
Harvard
Leitner, A, Maier-Kiener, V & Kiener, D 2018, 'High Temperature Flow Behavior of Ultra-Strong Nanoporous Au assessed by Spherical Nanoindentation', Nanomaterials, vol. 8.2018, no. 6, 366, pp. 1-12. https://doi.org/10.3390/nano8060366
APA
Vancouver
Leitner A, Maier-Kiener V, Kiener D. High Temperature Flow Behavior of Ultra-Strong Nanoporous Au assessed by Spherical Nanoindentation. Nanomaterials. 2018 May 24;8.2018(6):1-12. 366. doi: 10.3390/nano8060366
Author
Bibtex - Download
@article{33f22831fbdb402784dbf69a0bfd4c5b,
title = "High Temperature Flow Behavior of Ultra-Strong Nanoporous Au assessed by Spherical Nanoindentation",
author = "Alexander Leitner and Verena Maier-Kiener and Daniel Kiener",
year = "2018",
month = may,
day = "24",
doi = "10.3390/nano8060366",
language = "English",
volume = "8.2018",
pages = "1--12",
journal = "Nanomaterials",
issn = "2079-4991",
publisher = "Multidisciplinary Digital Publishing Institute (MDPI)",
number = "6",
}
RIS (suitable for import to EndNote) - Download
TY - JOUR
T1 - High Temperature Flow Behavior of Ultra-Strong Nanoporous Au assessed by Spherical Nanoindentation
AU - Leitner, Alexander
AU - Maier-Kiener, Verena
AU - Kiener, Daniel
PY - 2018/5/24
Y1 - 2018/5/24
U2 - 10.3390/nano8060366
DO - 10.3390/nano8060366
M3 - Article
VL - 8.2018
SP - 1
EP - 12
JO - Nanomaterials
JF - Nanomaterials
SN - 2079-4991
IS - 6
M1 - 366
ER -