Fractographic and Fracture Mechanical Invstigations of Refractories under Different Loading Conditions
Research output: Contribution to journal › Article › Research › peer-review
Authors
Organisational units
Details
Translated title of the contribution | Fractographic and Fracture Mechanical Invstigations of Refractories under Different Loading Conditions |
---|---|
Original language | English |
Pages (from-to) | 19-23 |
Journal | China's refractories |
Volume | 23 |