Environmental hydrogen embrittlement associated with decohesion and void formation at soluble coarse particles in a cold-rolled Al–Cu based alloy
Research output: Contribution to journal › Article › Research › peer-review
Standard
In: Materials science and engineering: A, Structural materials: properties, microstructure and processing, Vol. 799.2022, No. 2 January, 139850, 09.07.2020.
Research output: Contribution to journal › Article › Research › peer-review
Harvard
APA
Vancouver
Author
Bibtex - Download
}
RIS (suitable for import to EndNote) - Download
TY - JOUR
T1 - Environmental hydrogen embrittlement associated with decohesion and void formation at soluble coarse particles in a cold-rolled Al–Cu based alloy
AU - Safyari, Mahdieh
AU - Moshtaghi, Masoud
AU - Kuramoto, Shigeru
PY - 2020/7/9
Y1 - 2020/7/9
UR - http://dx.doi.org/10.1016/j.msea.2020.139850
U2 - 10.1016/j.msea.2020.139850
DO - 10.1016/j.msea.2020.139850
M3 - Article
VL - 799.2022
JO - Materials science and engineering: A, Structural materials: properties, microstructure and processing
JF - Materials science and engineering: A, Structural materials: properties, microstructure and processing
SN - 0921-5093
IS - 2 January
M1 - 139850
ER -