Effect of weld defects on the fatigue strength of ultra high-strength steels
Research output: Contribution to journal › Article › Research › peer-review
Authors
Organisational units
Details
Original language | English |
---|---|
Pages (from-to) | 214-222 |
Journal | Procedia Engineering |
Issue number | 160 |
Publication status | Published - 2016 |