Comprehensive investigation of the viscoelastic properties of PMMA by nanoindentation

Research output: Contribution to journalArticleResearchpeer-review

Standard

Comprehensive investigation of the viscoelastic properties of PMMA by nanoindentation. / Christöfl, Petra; Czibula, Caterina; Berer, Michael et al.
In: Polymer Testing, Vol. 93.2021, No. January, 106978, 27.11.2020.

Research output: Contribution to journalArticleResearchpeer-review

Vancouver

Christöfl P, Czibula C, Berer M, Oreski G, Teichert C, Pinter G. Comprehensive investigation of the viscoelastic properties of PMMA by nanoindentation. Polymer Testing. 2020 Nov 27;93.2021(January):106978. doi: 10.1016/j.polymertesting.2020.106978

Author

Christöfl, Petra ; Czibula, Caterina ; Berer, Michael et al. / Comprehensive investigation of the viscoelastic properties of PMMA by nanoindentation. In: Polymer Testing. 2020 ; Vol. 93.2021, No. January.

Bibtex - Download

@article{2c0fa3c65fb443e2b45af8ceaa1a7007,
title = "Comprehensive investigation of the viscoelastic properties of PMMA by nanoindentation",
keywords = "AFM, Amorphous, Compression test, Creep, Nanoindentation, viscoelastic properties of PMMA",
author = "Petra Christ{\"o}fl and Caterina Czibula and Michael Berer and Gernot Oreski and Christian Teichert and Gerald Pinter",
year = "2020",
month = nov,
day = "27",
doi = "10.1016/j.polymertesting.2020.106978",
language = "English",
volume = "93.2021",
journal = "Polymer Testing",
issn = "0142-9418",
publisher = "Elsevier Ltd",
number = "January",

}

RIS (suitable for import to EndNote) - Download

TY - JOUR

T1 - Comprehensive investigation of the viscoelastic properties of PMMA by nanoindentation

AU - Christöfl, Petra

AU - Czibula, Caterina

AU - Berer, Michael

AU - Oreski, Gernot

AU - Teichert, Christian

AU - Pinter, Gerald

PY - 2020/11/27

Y1 - 2020/11/27

KW - AFM

KW - Amorphous

KW - Compression test

KW - Creep

KW - Nanoindentation

KW - viscoelastic properties of PMMA

UR - http://www.scopus.com/inward/record.url?scp=85097371877&partnerID=8YFLogxK

U2 - 10.1016/j.polymertesting.2020.106978

DO - 10.1016/j.polymertesting.2020.106978

M3 - Article

AN - SCOPUS:85097371877

VL - 93.2021

JO - Polymer Testing

JF - Polymer Testing

SN - 0142-9418

IS - January

M1 - 106978

ER -