Characterization of delta-phase in superalloy Allvac 718Plus TM

Research output: Contribution to journalArticleResearchpeer-review

Standard

Characterization of delta-phase in superalloy Allvac 718Plus TM. / Stotter, Christoph; Sommitsch, Christof; Wagner, Julian et al.
In: International journal of materials research : IJMR ; Zeitschrift für Metallkunde, Vol. 99, 2008, p. 376-380.

Research output: Contribution to journalArticleResearchpeer-review

Bibtex - Download

@article{541738820d534f229a651f5c2dabe148,
title = "Characterization of delta-phase in superalloy Allvac 718Plus TM",
author = "Christoph Stotter and Christof Sommitsch and Julian Wagner and Harald Leitner and Ilse Letofsky-Papst and Gerald Zickler and Werner Prantl and Martin Stockinger",
year = "2008",
language = "English",
volume = "99",
pages = "376--380",
journal = "International journal of materials research : IJMR ; Zeitschrift f{\"u}r Metallkunde",
issn = "1862-5282",
publisher = "Walter de Gruyter GmbH",

}

RIS (suitable for import to EndNote) - Download

TY - JOUR

T1 - Characterization of delta-phase in superalloy Allvac 718Plus TM

AU - Stotter, Christoph

AU - Sommitsch, Christof

AU - Wagner, Julian

AU - Leitner, Harald

AU - Letofsky-Papst, Ilse

AU - Zickler, Gerald

AU - Prantl, Werner

AU - Stockinger, Martin

PY - 2008

Y1 - 2008

M3 - Article

VL - 99

SP - 376

EP - 380

JO - International journal of materials research : IJMR ; Zeitschrift für Metallkunde

JF - International journal of materials research : IJMR ; Zeitschrift für Metallkunde

SN - 1862-5282

ER -