A comparison of microstructure and casting defects of rheocasting and thixocasting Al-Si-Mg alloys

Research output: Chapter in Book/Report/Conference proceedingChapterResearch

Standard

A comparison of microstructure and casting defects of rheocasting and thixocasting Al-Si-Mg alloys. / LI, Jiehua; Spáčil, Ivo; Winklhofer, Johannes et al.
Solid State Phenomena. Vol. 347 2023. p. 61-66 (Solid State Phenomena).

Research output: Chapter in Book/Report/Conference proceedingChapterResearch

Harvard

LI, J, Spáčil, I, Winklhofer, J, Hofstätter, F & Griesebner, S 2023, A comparison of microstructure and casting defects of rheocasting and thixocasting Al-Si-Mg alloys. in Solid State Phenomena. vol. 347, Solid State Phenomena, pp. 61-66.

APA

LI, J., Spáčil, I., Winklhofer, J., Hofstätter, F., & Griesebner, S. (2023). A comparison of microstructure and casting defects of rheocasting and thixocasting Al-Si-Mg alloys. In Solid State Phenomena (Vol. 347, pp. 61-66). (Solid State Phenomena).

Vancouver

LI J, Spáčil I, Winklhofer J, Hofstätter F, Griesebner S. A comparison of microstructure and casting defects of rheocasting and thixocasting Al-Si-Mg alloys. In Solid State Phenomena. Vol. 347. 2023. p. 61-66. (Solid State Phenomena).

Author

LI, Jiehua ; Spáčil, Ivo ; Winklhofer, Johannes et al. / A comparison of microstructure and casting defects of rheocasting and thixocasting Al-Si-Mg alloys. Solid State Phenomena. Vol. 347 2023. pp. 61-66 (Solid State Phenomena).

Bibtex - Download

@inbook{59976d2f08a940f19cd0d16e4187efb3,
title = "A comparison of microstructure and casting defects of rheocasting and thixocasting Al-Si-Mg alloys",
author = "Jiehua LI and Ivo Sp{\'a}{\v c}il and Johannes Winklhofer and Fabian Hofst{\"a}tter and Stefan Griesebner",
year = "2023",
language = "English",
volume = "347",
series = "Solid State Phenomena",
publisher = "Trans Tech Publications",
pages = "61--66",
booktitle = "Solid State Phenomena",

}

RIS (suitable for import to EndNote) - Download

TY - CHAP

T1 - A comparison of microstructure and casting defects of rheocasting and thixocasting Al-Si-Mg alloys

AU - LI, Jiehua

AU - Spáčil, Ivo

AU - Winklhofer, Johannes

AU - Hofstätter, Fabian

AU - Griesebner, Stefan

PY - 2023

Y1 - 2023

M3 - Chapter

VL - 347

T3 - Solid State Phenomena

SP - 61

EP - 66

BT - Solid State Phenomena

ER -