Fractography of 3D-printed alumina ceramics tested in different printing directions
Activity: Talk or presentation › Oral presentation
Participants
- Josef Christian Schlacher - Speaker
- Anna-Katharina Hofer - contributor
- Irina Rosenova Kraleva - contributor
- Tanja Lube - contributor
- Martin Schwentenwein - contributor
- Raul Bermejo - contributor
Date
8 Feb 2021
Josef Christian Schlacher - Speaker
Anna-Katharina Hofer - contributor
Irina Rosenova Kraleva - contributor
Tanja Lube - contributor
Martin Schwentenwein - contributor
Raul Bermejo - contributor
8 Feb 2021
Event (Conference)
Title | Virtual 45<sup>th </sup>International Conference and Expo on Advanced Ceramics and Composites 2021 |
---|---|
Period | 8/02/21 → 12/02/21 |
Degree of recognition | International event |