Transmission electron microscopy of single and double aged 718plus superalloy

Publikationen: Beitrag in FachzeitschriftArtikelForschung(peer-reviewed)

Standard

Transmission electron microscopy of single and double aged 718plus superalloy. / Whitmore, Lawrence; Leitner, Harald; Povoden-Karadeniz, Erwin et al.
in: Materials science and engineering: A, Structural materials: properties, microstructure and processing, Jahrgang 534, 2012, S. 413-423.

Publikationen: Beitrag in FachzeitschriftArtikelForschung(peer-reviewed)

Bibtex - Download

@article{50c9661c798e46059f2515d58e9c83a9,
title = "Transmission electron microscopy of single and double aged 718plus superalloy",
author = "Lawrence Whitmore and Harald Leitner and Erwin Povoden-Karadeniz and Rene Radis and Martin Stockinger",
year = "2012",
doi = "10.10167j.msea.2011.11.089",
language = "English",
volume = "534",
pages = "413--423",
journal = "Materials science and engineering: A, Structural materials: properties, microstructure and processing",
issn = "0921-5093",
publisher = "Elsevier Ltd",

}

RIS (suitable for import to EndNote) - Download

TY - JOUR

T1 - Transmission electron microscopy of single and double aged 718plus superalloy

AU - Whitmore, Lawrence

AU - Leitner, Harald

AU - Povoden-Karadeniz, Erwin

AU - Radis, Rene

AU - Stockinger, Martin

PY - 2012

Y1 - 2012

U2 - 10.10167j.msea.2011.11.089

DO - 10.10167j.msea.2011.11.089

M3 - Article

VL - 534

SP - 413

EP - 423

JO - Materials science and engineering: A, Structural materials: properties, microstructure and processing

JF - Materials science and engineering: A, Structural materials: properties, microstructure and processing

SN - 0921-5093

ER -