Strength and Fractography of High Power Varistors

Publikationen: Beitrag in Buch/Bericht/KonferenzbandBeitrag in Buch/SammelbandForschung

Standard

Strength and Fractography of High Power Varistors. / Supancic, Peter; Wang, Zhonghua; Aldrian, F. et al.
Key engineering materials. 2005. S. 358-365 (Key engineering materials).

Publikationen: Beitrag in Buch/Bericht/KonferenzbandBeitrag in Buch/SammelbandForschung

Harvard

Supancic, P, Wang, Z, Aldrian, F, Schriener, A & Danzer, R 2005, Strength and Fractography of High Power Varistors. in Key engineering materials. Key engineering materials, S. 358-365.

APA

Supancic, P., Wang, Z., Aldrian, F., Schriener, A., & Danzer, R. (2005). Strength and Fractography of High Power Varistors. In Key engineering materials (S. 358-365). (Key engineering materials).

Vancouver

Supancic P, Wang Z, Aldrian F, Schriener A, Danzer R. Strength and Fractography of High Power Varistors. in Key engineering materials. 2005. S. 358-365. (Key engineering materials).

Author

Supancic, Peter ; Wang, Zhonghua ; Aldrian, F. et al. / Strength and Fractography of High Power Varistors. Key engineering materials. 2005. S. 358-365 (Key engineering materials).

Bibtex - Download

@inbook{dd4da0d79d5141119291eb46a0053bd4,
title = "Strength and Fractography of High Power Varistors",
author = "Peter Supancic and Zhonghua Wang and F. Aldrian and A. Schriener and Robert Danzer",
year = "2005",
language = "English",
series = "Key engineering materials",
publisher = "Trans Tech Publications",
pages = "358--365",
booktitle = "Key engineering materials",

}

RIS (suitable for import to EndNote) - Download

TY - CHAP

T1 - Strength and Fractography of High Power Varistors

AU - Supancic, Peter

AU - Wang, Zhonghua

AU - Aldrian, F.

AU - Schriener, A.

AU - Danzer, Robert

PY - 2005

Y1 - 2005

M3 - Chapter

T3 - Key engineering materials

SP - 358

EP - 365

BT - Key engineering materials

ER -