Spray forming and post processing of superalloy rings
Publikationen: Konferenzbeitrag › Paper › (peer-reviewed)
Standard
2005. 429-440 Beitrag in 6th International Symposium on Superalloys 718, 625, 706 and Derivatives, Pittsburgh, PA, USA / Vereinigte Staaten.
Publikationen: Konferenzbeitrag › Paper › (peer-reviewed)
Harvard
APA
Vancouver
Author
Bibtex - Download
}
RIS (suitable for import to EndNote) - Download
TY - CONF
T1 - Spray forming and post processing of superalloy rings
AU - Walter, Michael
AU - Stockinger, Martin
AU - Tockner, Johann
AU - Ellendt, Nils
AU - Uhlenwinkel, Volker
PY - 2005
Y1 - 2005
KW - Forging
KW - Hot isostatic pressing
KW - Microstructure evaluation
KW - Spray forming
UR - http://www.scopus.com/inward/record.url?scp=33644851113&partnerID=8YFLogxK
U2 - 10.7449/2005/superalloys_2005_429_440
DO - 10.7449/2005/superalloys_2005_429_440
M3 - Paper
AN - SCOPUS:33644851113
SP - 429
EP - 440
T2 - 6th International Symposium on Superalloys 718, 625, 706 and Derivatives
Y2 - 2 October 2005 through 5 October 2005
ER -