Revealing deformation mechanisms in small dimensions with micro-compression and nanoindentation tests
Publikationen: Konferenzbeitrag › Poster › Forschung › (peer-reviewed)
Standard
Revealing deformation mechanisms in small dimensions with micro-compression and nanoindentation tests. / Rester, Martin; Kirchlechner, Christoph; Motz, Christian et al.
2009. Postersitzung präsentiert bei Microscopy Conference 2009, Graz, Österreich.
2009. Postersitzung präsentiert bei Microscopy Conference 2009, Graz, Österreich.
Publikationen: Konferenzbeitrag › Poster › Forschung › (peer-reviewed)
Harvard
Rester, M, Kirchlechner, C, Motz, C, Pippan, R, Clemens, H & Dehm, G 2009, 'Revealing deformation mechanisms in small dimensions with micro-compression and nanoindentation tests', Microscopy Conference 2009, Graz, Österreich, 30/08/09 - 4/09/09.
APA
Rester, M., Kirchlechner, C., Motz, C., Pippan, R., Clemens, H., & Dehm, G. (2009). Revealing deformation mechanisms in small dimensions with micro-compression and nanoindentation tests. Postersitzung präsentiert bei Microscopy Conference 2009, Graz, Österreich.
Vancouver
Rester M, Kirchlechner C, Motz C, Pippan R, Clemens H, Dehm G. Revealing deformation mechanisms in small dimensions with micro-compression and nanoindentation tests. 2009. Postersitzung präsentiert bei Microscopy Conference 2009, Graz, Österreich.
Author
Bibtex - Download
@conference{430818b759714618a8d53669ed340e63,
title = "Revealing deformation mechanisms in small dimensions with micro-compression and nanoindentation tests",
author = "Martin Rester and Christoph Kirchlechner and Christian Motz and Reinhard Pippan and Helmut Clemens and Gerhard Dehm",
year = "2009",
language = "English",
note = "Microscopy Conference 2009 ; Conference date: 30-08-2009 Through 04-09-2009",
}
RIS (suitable for import to EndNote) - Download
TY - CONF
T1 - Revealing deformation mechanisms in small dimensions with micro-compression and nanoindentation tests
AU - Rester, Martin
AU - Kirchlechner, Christoph
AU - Motz, Christian
AU - Pippan, Reinhard
AU - Clemens, Helmut
AU - Dehm, Gerhard
PY - 2009
Y1 - 2009
M3 - Poster
T2 - Microscopy Conference 2009
Y2 - 30 August 2009 through 4 September 2009
ER -