δ-Phase characterization of superalloy allvac 718 PlusTM

Publikationen: Beitrag in Buch/Bericht/KonferenzbandBeitrag in Konferenzband

Standard

δ-Phase characterization of superalloy allvac 718 PlusTM. / Sommitsch, Christof; Stotter, C.; Leitner, Harald et al.
TMS 2008. 2008. S. 1-6.

Publikationen: Beitrag in Buch/Bericht/KonferenzbandBeitrag in Konferenzband

Harvard

Sommitsch, C, Stotter, C, Leitner, H, Mitsche, S, Letofsky-Papst, I & Stockinger, M 2008, δ-Phase characterization of superalloy allvac 718 PlusTM. in TMS 2008. S. 1-6.

APA

Sommitsch, C., Stotter, C., Leitner, H., Mitsche, S., Letofsky-Papst, I., & Stockinger, M. (2008). δ-Phase characterization of superalloy allvac 718 PlusTM. In TMS 2008 (S. 1-6)

Vancouver

Sommitsch C, Stotter C, Leitner H, Mitsche S, Letofsky-Papst I, Stockinger M. δ-Phase characterization of superalloy allvac 718 PlusTM. in TMS 2008. 2008. S. 1-6

Bibtex - Download

@inproceedings{94c3fd57b9db40a6b6ea16675aa187e4,
title = "δ-Phase characterization of superalloy allvac 718 PlusTM",
author = "Christof Sommitsch and C. Stotter and Harald Leitner and S. Mitsche and I. Letofsky-Papst and M. Stockinger",
year = "2008",
language = "English",
pages = "1--6",
booktitle = "TMS 2008",

}

RIS (suitable for import to EndNote) - Download

TY - GEN

T1 - δ-Phase characterization of superalloy allvac 718 PlusTM

AU - Sommitsch, Christof

AU - Stotter, C.

AU - Leitner, Harald

AU - Mitsche, S.

AU - Letofsky-Papst, I.

AU - Stockinger, M.

PY - 2008

Y1 - 2008

M3 - Conference contribution

SP - 1

EP - 6

BT - TMS 2008

ER -