Overview of the Grain Size Effects on the Mechanical and Deformation Behaviour of Electrodeposited Nanocrystalline Nickel - from Nanoindentation to High Pressure Torsion
Publikationen: Beitrag in Fachzeitschrift › Artikel › Forschung › (peer-reviewed)
Standard
Overview of the Grain Size Effects on the Mechanical and Deformation Behaviour of Electrodeposited Nanocrystalline Nickel - from Nanoindentation to High Pressure Torsion. / Pippan, Reinhard; Yang, B.; Vehoff, H.
in: Materials Science Forum , 2010, S. 85-98.
in: Materials Science Forum , 2010, S. 85-98.
Publikationen: Beitrag in Fachzeitschrift › Artikel › Forschung › (peer-reviewed)
Harvard
Pippan, R, Yang, B & Vehoff, H 2010, 'Overview of the Grain Size Effects on the Mechanical and Deformation Behaviour of Electrodeposited Nanocrystalline Nickel - from Nanoindentation to High Pressure Torsion', Materials Science Forum , S. 85-98.
APA
Pippan, R., Yang, B., & Vehoff, H. (2010). Overview of the Grain Size Effects on the Mechanical and Deformation Behaviour of Electrodeposited Nanocrystalline Nickel - from Nanoindentation to High Pressure Torsion. Materials Science Forum , 85-98.
Vancouver
Author
Bibtex - Download
@article{0af016a91684490383c4bf556f25082e,
title = "Overview of the Grain Size Effects on the Mechanical and Deformation Behaviour of Electrodeposited Nanocrystalline Nickel - from Nanoindentation to High Pressure Torsion",
author = "Reinhard Pippan and B. Yang and H. Vehoff",
year = "2010",
language = "English",
pages = "85--98",
journal = "Materials Science Forum ",
issn = "0255-5476",
publisher = "Trans Tech Publications Ltd",
}
RIS (suitable for import to EndNote) - Download
TY - JOUR
T1 - Overview of the Grain Size Effects on the Mechanical and Deformation Behaviour of Electrodeposited Nanocrystalline Nickel - from Nanoindentation to High Pressure Torsion
AU - Pippan, Reinhard
AU - Yang, B.
AU - Vehoff, H.
PY - 2010
Y1 - 2010
M3 - Article
SP - 85
EP - 98
JO - Materials Science Forum
JF - Materials Science Forum
SN - 0255-5476
ER -