Numerical study on the formation of spurious grains and freckles during the directional solidification of superalloys

Publikationen: KonferenzbeitragPaper(peer-reviewed)

Externe Organisationseinheiten

  • Central South University, Changsha
  • Wedge Central South Research Institute

Abstract

Freckles, a significant issue encountered during the directional solidification of superal-
loys, are recognised by a trail of equiaxed grains parallel to the direction of gravity accompanied by
local eutectic enrichment. In the current study, a mixed-columnar-equiaxed multiphase volume-av-
erage solidification model was employed to study the formation of freckles in superalloy casting.
Fragments produced via flow-driven and capillary-driven fragmentation mechanisms are considered
as the source of spurious grains. The transport and the growth/remelting of the fragments are consid-
ered. According to the simulation results, some segregation channels develop at the corners of the
casting. Flow-driven fragments are produced in/around the segregation channels, whereas capillary-
driven fragments are produced at a certain depth of the mushy zone across the entire section of the
casting. The fragmentation rate caused by the flow-driven mechanism is several orders of magnitude
larger than that caused by the capillary-driven mechanism, i.e. the flow-driven fragmentation mech-
anism is dominant for the currently investigated sample. After the solidification process, four freckles
formed at the casting corners on the shadowed side, whereas it was freckle-free on the bright side.

Details

OriginalspracheEnglisch
Seitenumfang11
DOIs
StatusVeröffentlicht - 2023
VeranstaltungMCWASP XVI IOP Conf. Series: Materials Science and Engineering -
Dauer: 18 Juni 202323 Juni 2023

Konferenz

KonferenzMCWASP XVI IOP Conf. Series: Materials Science and Engineering
Zeitraum18/06/2323/06/23