Mechanical Properties of the Collagen/Mineral Composite in Bone - Study of Osteoporosis and Osteogenesis Imperfecta by a Combination of Nanoindentation and Quantitative Electron Backscattering

Publikationen: Thesis / Studienabschlussarbeiten und HabilitationsschriftenDissertation

Bibtex - Download

@phdthesis{f6a4ddd830864c2785cadc89f69ddcea,
title = "Mechanical Properties of the Collagen/Mineral Composite in Bone - Study of Osteoporosis and Osteogenesis Imperfecta by a Combination of Nanoindentation and Quantitative Electron Backscattering",
author = "Markus Weber",
note = "embargoed until null",
year = "2005",
language = "English",

}