Mechanical properties and deformation of CrN and Cr/CrN coatings during nanoindentation: Experiments and theoretical calculations
Publikationen: Beitrag in Buch/Bericht/Konferenzband › Beitrag in Konferenzband
Autoren
Organisationseinheiten
Details
Titel in Übersetzung | Mechanical properties and deformation of CrN and Cr/CrN coatings during nanoindentation: Experiments and theoretical calculations |
---|---|
Originalsprache | Englisch |
Titel | 35th International Conference on Metallurgical Coatings and Thin Films |
Seiten | 109-109 |