Investigation of the slow crack growth behavior of static and cyclic loaded specimens of polyethylene by 2D and 3D optical fracture surface analysis
Publikationen: Konferenzbeitrag › Poster › Forschung › (peer-reviewed)
Standard
Investigation of the slow crack growth behavior of static and cyclic loaded specimens of polyethylene by 2D and 3D optical fracture surface analysis. / Frank, Andreas; Bruckmoser, Katharina; Redhead, Anita et al.
2010. Postersitzung präsentiert bei 10th Austrian Polymer Meeting and 2nd Joint Austrian-Slovenian Polymer Meeting 2010, Leoben, Österreich.
2010. Postersitzung präsentiert bei 10th Austrian Polymer Meeting and 2nd Joint Austrian-Slovenian Polymer Meeting 2010, Leoben, Österreich.
Publikationen: Konferenzbeitrag › Poster › Forschung › (peer-reviewed)
Harvard
Frank, A, Bruckmoser, K, Redhead, A, Gruber, D & Pinter, G 2010, 'Investigation of the slow crack growth behavior of static and cyclic loaded specimens of polyethylene by 2D and 3D optical fracture surface analysis', 10th Austrian Polymer Meeting and 2nd Joint Austrian-Slovenian Polymer Meeting 2010, Leoben, Österreich, 8/09/10 - 10/09/10.
APA
Frank, A., Bruckmoser, K., Redhead, A., Gruber, D., & Pinter, G. (2010). Investigation of the slow crack growth behavior of static and cyclic loaded specimens of polyethylene by 2D and 3D optical fracture surface analysis. Postersitzung präsentiert bei 10th Austrian Polymer Meeting and 2nd Joint Austrian-Slovenian Polymer Meeting 2010, Leoben, Österreich.
Vancouver
Frank A, Bruckmoser K, Redhead A, Gruber D, Pinter G. Investigation of the slow crack growth behavior of static and cyclic loaded specimens of polyethylene by 2D and 3D optical fracture surface analysis. 2010. Postersitzung präsentiert bei 10th Austrian Polymer Meeting and 2nd Joint Austrian-Slovenian Polymer Meeting 2010, Leoben, Österreich.
Author
Bibtex - Download
@conference{eb909b394b3245baafb33886c0cca197,
title = "Investigation of the slow crack growth behavior of static and cyclic loaded specimens of polyethylene by 2D and 3D optical fracture surface analysis",
author = "Andreas Frank and Katharina Bruckmoser and Anita Redhead and Dieter Gruber and Gerald Pinter",
year = "2010",
language = "English",
note = "ASPM ; Conference date: 08-09-2010 Through 10-09-2010",
}
RIS (suitable for import to EndNote) - Download
TY - CONF
T1 - Investigation of the slow crack growth behavior of static and cyclic loaded specimens of polyethylene by 2D and 3D optical fracture surface analysis
AU - Frank, Andreas
AU - Bruckmoser, Katharina
AU - Redhead, Anita
AU - Gruber, Dieter
AU - Pinter, Gerald
PY - 2010
Y1 - 2010
M3 - Poster
T2 - ASPM
Y2 - 8 September 2010 through 10 September 2010