Insights into the deformation behavior of the CrMnFeCoNi high-entropy alloy revealed by elevated temperature nanoindentation

Publikationen: Beitrag in FachzeitschriftArtikelForschung(peer-reviewed)

Standard

Insights into the deformation behavior of the CrMnFeCoNi high-entropy alloy revealed by elevated temperature nanoindentation. / Maier-Kiener, Verena; Schuh, Benjamin; George, Easo P. et al.
in: Journal of materials research (JMR), Jahrgang 32.2017, Nr. 14, 01.07.2017, S. 2658-2667.

Publikationen: Beitrag in FachzeitschriftArtikelForschung(peer-reviewed)

Bibtex - Download

@article{e08fe5ff669446ee8185f462599bcf51,
title = "Insights into the deformation behavior of the CrMnFeCoNi high-entropy alloy revealed by elevated temperature nanoindentation",
author = "Verena Maier-Kiener and Benjamin Schuh and George, {Easo P.} and Helmut Clemens and Anton Hohenwarter",
year = "2017",
month = jul,
day = "1",
doi = "10.1557/jmr.2017.260",
language = "English",
volume = "32.2017",
pages = "2658--2667",
journal = "Journal of materials research (JMR)",
issn = "0884-2914",
publisher = "Springer International Publishing",
number = "14",

}

RIS (suitable for import to EndNote) - Download

TY - JOUR

T1 - Insights into the deformation behavior of the CrMnFeCoNi high-entropy alloy revealed by elevated temperature nanoindentation

AU - Maier-Kiener, Verena

AU - Schuh, Benjamin

AU - George, Easo P.

AU - Clemens, Helmut

AU - Hohenwarter, Anton

PY - 2017/7/1

Y1 - 2017/7/1

U2 - 10.1557/jmr.2017.260

DO - 10.1557/jmr.2017.260

M3 - Article

VL - 32.2017

SP - 2658

EP - 2667

JO - Journal of materials research (JMR)

JF - Journal of materials research (JMR)

SN - 0884-2914

IS - 14

ER -