Galvanic corrosion and stress corrosion cracking of steel and aluminium bolts in magnesium die cast alloy AZ91
Publikationen: Beitrag in Buch/Bericht/Konferenzband › Beitrag in Konferenzband
Standard
Galvanic corrosion and stress corrosion cracking of steel and aluminium bolts in magnesium die cast alloy AZ91. / Gerstmayr, Gerhard; Mori, Gregor; Eichlseder, Wilfried.
Magnesium Technology 2010. 2010. S. 145-150.
Magnesium Technology 2010. 2010. S. 145-150.
Publikationen: Beitrag in Buch/Bericht/Konferenzband › Beitrag in Konferenzband
Harvard
Gerstmayr, G, Mori, G & Eichlseder, W 2010, Galvanic corrosion and stress corrosion cracking of steel and aluminium bolts in magnesium die cast alloy AZ91. in Magnesium Technology 2010. S. 145-150.
APA
Gerstmayr, G., Mori, G., & Eichlseder, W. (2010). Galvanic corrosion and stress corrosion cracking of steel and aluminium bolts in magnesium die cast alloy AZ91. In Magnesium Technology 2010 (S. 145-150)
Vancouver
Gerstmayr G, Mori G, Eichlseder W. Galvanic corrosion and stress corrosion cracking of steel and aluminium bolts in magnesium die cast alloy AZ91. in Magnesium Technology 2010. 2010. S. 145-150
Author
Bibtex - Download
@inproceedings{bf08a3db3e8e4a96832f105f36aa6e4b,
title = "Galvanic corrosion and stress corrosion cracking of steel and aluminium bolts in magnesium die cast alloy AZ91",
author = "Gerhard Gerstmayr and Gregor Mori and Wilfried Eichlseder",
year = "2010",
language = "English",
pages = "145--150",
booktitle = "Magnesium Technology 2010",
}
RIS (suitable for import to EndNote) - Download
TY - GEN
T1 - Galvanic corrosion and stress corrosion cracking of steel and aluminium bolts in magnesium die cast alloy AZ91
AU - Gerstmayr, Gerhard
AU - Mori, Gregor
AU - Eichlseder, Wilfried
PY - 2010
Y1 - 2010
M3 - Conference contribution
SP - 145
EP - 150
BT - Magnesium Technology 2010
ER -