Fractography of Thermistors

Publikationen: Beitrag in Buch/Bericht/KonferenzbandBeitrag in Buch/SammelbandForschung

Standard

Fractography of Thermistors. / Danzer, Robert; Platzer, Alexander; Supancic, Peter et al.
Fractography of Glasses and Ceramics V. 2007. S. 231-242.

Publikationen: Beitrag in Buch/Bericht/KonferenzbandBeitrag in Buch/SammelbandForschung

Harvard

Danzer, R, Platzer, A, Supancic, P & Wang, Z 2007, Fractography of Thermistors. in Fractography of Glasses and Ceramics V. S. 231-242.

APA

Danzer, R., Platzer, A., Supancic, P., & Wang, Z. (2007). Fractography of Thermistors. In Fractography of Glasses and Ceramics V (S. 231-242)

Vancouver

Danzer R, Platzer A, Supancic P, Wang Z. Fractography of Thermistors. in Fractography of Glasses and Ceramics V. 2007. S. 231-242

Author

Danzer, Robert ; Platzer, Alexander ; Supancic, Peter et al. / Fractography of Thermistors. Fractography of Glasses and Ceramics V. 2007. S. 231-242

Bibtex - Download

@inbook{692f7eea5c9745e4bae2ae64c9f3b7de,
title = "Fractography of Thermistors",
author = "Robert Danzer and Alexander Platzer and Peter Supancic and Zhonghua Wang",
year = "2007",
language = "English",
pages = "231--242",
booktitle = "Fractography of Glasses and Ceramics V",

}

RIS (suitable for import to EndNote) - Download

TY - CHAP

T1 - Fractography of Thermistors

AU - Danzer, Robert

AU - Platzer, Alexander

AU - Supancic, Peter

AU - Wang, Zhonghua

PY - 2007

Y1 - 2007

M3 - Chapter

SP - 231

EP - 242

BT - Fractography of Glasses and Ceramics V

ER -