Fractographic and fracture mechanical investigations of refractories under different loading conditions
Publikationen: Beitrag in Buch/Bericht/Konferenzband › Beitrag in Konferenzband
Standard
Fractographic and fracture mechanical investigations of refractories under different loading conditions. / Harmuth, Harald; Tschegg, E.K.
Proceedings of the 6th international symposium on refractories. 2012. S. 485-488.
Proceedings of the 6th international symposium on refractories. 2012. S. 485-488.
Publikationen: Beitrag in Buch/Bericht/Konferenzband › Beitrag in Konferenzband
Harvard
Harmuth, H & Tschegg, EK 2012, Fractographic and fracture mechanical investigations of refractories under different loading conditions. in Proceedings of the 6th international symposium on refractories. S. 485-488.
APA
Harmuth, H., & Tschegg, E. K. (2012). Fractographic and fracture mechanical investigations of refractories under different loading conditions. In Proceedings of the 6th international symposium on refractories (S. 485-488)
Vancouver
Harmuth H, Tschegg EK. Fractographic and fracture mechanical investigations of refractories under different loading conditions. in Proceedings of the 6th international symposium on refractories. 2012. S. 485-488
Author
Bibtex - Download
@inproceedings{d55866e0a3d8412fad1b18c3522ce774,
title = "Fractographic and fracture mechanical investigations of refractories under different loading conditions",
author = "Harald Harmuth and E.K. Tschegg",
year = "2012",
language = "English",
isbn = "978-7-5645-1139-5",
pages = "485--488",
booktitle = "Proceedings of the 6th international symposium on refractories",
}
RIS (suitable for import to EndNote) - Download
TY - GEN
T1 - Fractographic and fracture mechanical investigations of refractories under different loading conditions
AU - Harmuth, Harald
AU - Tschegg, E.K.
PY - 2012
Y1 - 2012
M3 - Conference contribution
SN - 978-7-5645-1139-5
SP - 485
EP - 488
BT - Proceedings of the 6th international symposium on refractories
ER -