abstract = "This diploma thesis focuses on microstructure-related diffusion processes in selected arc evaporated face centered cubic (fcc) Ti-, fcc Cr- and hexagonal closed packed (hcp) Al-based nitride coatings, which are used as wear protective coatings for cutting processes. A comparative study of fcc Cr1-xAlxN (x=0, 0.7), fcc Ti1-xAlxN (x=0, 0.5, 0.6) and fcc TiCN coatings on cutting tools showed surprisingly superior wear behavior predominantly of the conventional coating systems, i.e. TiN and TiCN. The reason for that was found in diffusion processes at the elevated temperatures of cutting, contributing to degradation of the coating structure and thus to deteriorating cutting performance. In order to study diffusion processes in these coatings, coated high speed steel substrates were annealed at Ta=900, 1000, 1100, 1200 °C in vacuum for 3 hours and the elemental and phase composition of the coatings was subsequently studied by a combination of X-ray diffraction and backscattered electron imaging, elemental mapping with qualitative linescans and quantitative energy-dispersive X-ray spectroscopy. It is explained how diffusion processes are related to the decomposition routes of the metastable coatings, which are associated with the generation of diffusion paths promoting transport of elements through the coating. This is highly pronounced in metastable TiAlN, which decomposes to thermally stable hcp AlN and fcc TiN. Even much stronger diffusion is present in coatings undergoing two-step decomposition processes. This is typical for the metastable fcc CrAlN, which decomposes to thermally stable hcp AlN but unstable fcc CrN, which in turn decomposes further to Cr2N and Cr due to the release of weakly bonded N. This results in generation of efficient diffusion paths. On the other hand, the thermally stable TiN, TiCN or AlN represent effective diffusion barriers with only limited diffusion processes predominantly at the grain boundaries.",
keywords = "Diffusionsverschlei{\ss}, Verschlei{\ss}, Schneidwerkzeuge, Lichtbogenverdampfung, Diffusion, Eisendiffusion, metastabile Phasen, {\"U}bergangsmetallnitride, gl{\"u}hen, Zersetzung, Diffusionsbarriere, Phasen{\"u}bergang, Schnellarbeitsstahl, Zerspanung, Zerspanungswerkzeuge, Hochleistungszerspanung, high speed cutting, diffusion, diffusion into cutting tools, wear, diffusion wear, coatings, high speed steel, HSS, diffusional barriers, annealing, decomposition, CrN, AlN, Cr1-xAlxN, Ti1-xAlxN, TiN, TiCN, phase transformation, metastable coatings, arc evaporation",
author = "Ernst Plesiutschnig",
note = "embargoed until 22-11-2016",
year = "2011",
language = "English",
type = "Diploma Thesis",

}

RIS (suitable for import to EndNote) - Download

TY - THES

T1 - Fe diffusion in selected transition metal nitride coatings

AU - Plesiutschnig, Ernst

N1 - embargoed until 22-11-2016

PY - 2011

Y1 - 2011

N2 - This diploma thesis focuses on microstructure-related diffusion processes in selected arc evaporated face centered cubic (fcc) Ti-, fcc Cr- and hexagonal closed packed (hcp) Al-based nitride coatings, which are used as wear protective coatings for cutting processes. A comparative study of fcc Cr1-xAlxN (x=0, 0.7), fcc Ti1-xAlxN (x=0, 0.5, 0.6) and fcc TiCN coatings on cutting tools showed surprisingly superior wear behavior predominantly of the conventional coating systems, i.e. TiN and TiCN. The reason for that was found in diffusion processes at the elevated temperatures of cutting, contributing to degradation of the coating structure and thus to deteriorating cutting performance. In order to study diffusion processes in these coatings, coated high speed steel substrates were annealed at Ta=900, 1000, 1100, 1200 °C in vacuum for 3 hours and the elemental and phase composition of the coatings was subsequently studied by a combination of X-ray diffraction and backscattered electron imaging, elemental mapping with qualitative linescans and quantitative energy-dispersive X-ray spectroscopy. It is explained how diffusion processes are related to the decomposition routes of the metastable coatings, which are associated with the generation of diffusion paths promoting transport of elements through the coating. This is highly pronounced in metastable TiAlN, which decomposes to thermally stable hcp AlN and fcc TiN. Even much stronger diffusion is present in coatings undergoing two-step decomposition processes. This is typical for the metastable fcc CrAlN, which decomposes to thermally stable hcp AlN but unstable fcc CrN, which in turn decomposes further to Cr2N and Cr due to the release of weakly bonded N. This results in generation of efficient diffusion paths. On the other hand, the thermally stable TiN, TiCN or AlN represent effective diffusion barriers with only limited diffusion processes predominantly at the grain boundaries.

AB - This diploma thesis focuses on microstructure-related diffusion processes in selected arc evaporated face centered cubic (fcc) Ti-, fcc Cr- and hexagonal closed packed (hcp) Al-based nitride coatings, which are used as wear protective coatings for cutting processes. A comparative study of fcc Cr1-xAlxN (x=0, 0.7), fcc Ti1-xAlxN (x=0, 0.5, 0.6) and fcc TiCN coatings on cutting tools showed surprisingly superior wear behavior predominantly of the conventional coating systems, i.e. TiN and TiCN. The reason for that was found in diffusion processes at the elevated temperatures of cutting, contributing to degradation of the coating structure and thus to deteriorating cutting performance. In order to study diffusion processes in these coatings, coated high speed steel substrates were annealed at Ta=900, 1000, 1100, 1200 °C in vacuum for 3 hours and the elemental and phase composition of the coatings was subsequently studied by a combination of X-ray diffraction and backscattered electron imaging, elemental mapping with qualitative linescans and quantitative energy-dispersive X-ray spectroscopy. It is explained how diffusion processes are related to the decomposition routes of the metastable coatings, which are associated with the generation of diffusion paths promoting transport of elements through the coating. This is highly pronounced in metastable TiAlN, which decomposes to thermally stable hcp AlN and fcc TiN. Even much stronger diffusion is present in coatings undergoing two-step decomposition processes. This is typical for the metastable fcc CrAlN, which decomposes to thermally stable hcp AlN but unstable fcc CrN, which in turn decomposes further to Cr2N and Cr due to the release of weakly bonded N. This results in generation of efficient diffusion paths. On the other hand, the thermally stable TiN, TiCN or AlN represent effective diffusion barriers with only limited diffusion processes predominantly at the grain boundaries.

KW - Diffusionsverschleiß

KW - Verschleiß

KW - Schneidwerkzeuge

KW - Lichtbogenverdampfung

KW - Diffusion

KW - Eisendiffusion

KW - metastabile Phasen

KW - Übergangsmetallnitride

KW - glühen

KW - Zersetzung

KW - Diffusionsbarriere

KW - Phasenübergang

KW - Schnellarbeitsstahl

KW - Zerspanung

KW - Zerspanungswerkzeuge

KW - Hochleistungszerspanung

KW - high speed cutting

KW - diffusion

KW - diffusion into cutting tools

KW - wear

KW - diffusion wear

KW - coatings

KW - high speed steel

KW - HSS

KW - diffusional barriers

KW - annealing

KW - decomposition

KW - CrN

KW - AlN

KW - Cr1-xAlxN

KW - Ti1-xAlxN

KW - TiN

KW - TiCN

KW - phase transformation

KW - metastable coatings

KW - arc evaporation

M3 - Diploma Thesis

ER -