Effect of Eu and P additions with Ta grain refiner on the solidification microstructure of Al-7Si-0.3Mg alloys
Publikationen: Beitrag in Fachzeitschrift › Artikel › Forschung › (peer-reviewed)
Standard
in: IOP Conference Series: Materials Science and Engineering, Jahrgang 2023, Nr. 1274, 012006, 2023.
Publikationen: Beitrag in Fachzeitschrift › Artikel › Forschung › (peer-reviewed)
Harvard
APA
Vancouver
Author
Bibtex - Download
}
RIS (suitable for import to EndNote) - Download
TY - JOUR
T1 - Effect of Eu and P additions with Ta grain refiner on the solidification microstructure of Al-7Si-0.3Mg alloys
AU - Spacil, Ivo
AU - Schumacher, Peter
AU - LI, Jiehua
PY - 2023
Y1 - 2023
N2 - Al-7Si-0.3Mg based alloys have been widely used. Nevertheless, at least three issues during melt treatment (grain refinement of Al grains, modification of eutectic Si and refinement of eutectic grain size) need to be further explored. In this contribution, we focus on these three melt treatments. For grain refinement of Al grains, the stochiometric Al-2.2Ti-1B grain refiner rod together with 0.12 wt. % Ta was used. For modification of eutectic Si, Eu up to 500 ppm was used. The best modification can be obtained with 200 ppm Eu. By further increasing Eu up to 500 ppm, modification level becomes worse due to the formation of Al2Si2Eu. For the refinement of eutectic grain size, a combined addition of Eu (up to 500 ppm) and P (up to 40 ppm) was used. With increasing P concentration, the modification of eutectic Si became worse. The size of eutectic Si increases, the shape factor of eutectic Si decreases. When the P concentration is higher, more Eu is needed for a well-modified eutectic Si. This investigation provides a novel concept for melt treatment of Al-Si-Mg based alloys.
AB - Al-7Si-0.3Mg based alloys have been widely used. Nevertheless, at least three issues during melt treatment (grain refinement of Al grains, modification of eutectic Si and refinement of eutectic grain size) need to be further explored. In this contribution, we focus on these three melt treatments. For grain refinement of Al grains, the stochiometric Al-2.2Ti-1B grain refiner rod together with 0.12 wt. % Ta was used. For modification of eutectic Si, Eu up to 500 ppm was used. The best modification can be obtained with 200 ppm Eu. By further increasing Eu up to 500 ppm, modification level becomes worse due to the formation of Al2Si2Eu. For the refinement of eutectic grain size, a combined addition of Eu (up to 500 ppm) and P (up to 40 ppm) was used. With increasing P concentration, the modification of eutectic Si became worse. The size of eutectic Si increases, the shape factor of eutectic Si decreases. When the P concentration is higher, more Eu is needed for a well-modified eutectic Si. This investigation provides a novel concept for melt treatment of Al-Si-Mg based alloys.
U2 - 10.1088/1757-899X/1274/1/012006
DO - 10.1088/1757-899X/1274/1/012006
M3 - Article
VL - 2023
JO - IOP Conference Series: Materials Science and Engineering
JF - IOP Conference Series: Materials Science and Engineering
SN - 1757-8981
IS - 1274
M1 - 012006
ER -