Defect analysis in semicrystalline polymers using combined differential scanning calorimetry and X-ray line profile analysis
Publikationen: Konferenzbeitrag › Poster › Forschung › (peer-reviewed)
Standard
Defect analysis in semicrystalline polymers using combined differential scanning calorimetry and X-ray line profile analysis. / Spieckermann, Florian.
2016. Postersitzung präsentiert bei Lähnwitz Seminar on Calorimetry 2016 in Rostock, Rostock, Deutschland.
2016. Postersitzung präsentiert bei Lähnwitz Seminar on Calorimetry 2016 in Rostock, Rostock, Deutschland.
Publikationen: Konferenzbeitrag › Poster › Forschung › (peer-reviewed)
Harvard
Spieckermann, F 2016, 'Defect analysis in semicrystalline polymers using combined differential scanning calorimetry and X-ray line profile analysis', Lähnwitz Seminar on Calorimetry 2016 in Rostock, Rostock, Deutschland, 8/06/15 - 11/06/15.
APA
Spieckermann, F. (2016). Defect analysis in semicrystalline polymers using combined differential scanning calorimetry and X-ray line profile analysis. Postersitzung präsentiert bei Lähnwitz Seminar on Calorimetry 2016 in Rostock, Rostock, Deutschland.
Vancouver
Spieckermann F. Defect analysis in semicrystalline polymers using combined differential scanning calorimetry and X-ray line profile analysis. 2016. Postersitzung präsentiert bei Lähnwitz Seminar on Calorimetry 2016 in Rostock, Rostock, Deutschland.
Author
Bibtex - Download
@conference{73d56b11d3b54c9d962d174121e6d228,
title = "Defect analysis in semicrystalline polymers using combined differential scanning calorimetry and X-ray line profile analysis",
author = "Florian Spieckermann",
year = "2016",
month = jun,
language = "English",
note = "L{\"a}hnwitz Seminar on Calorimetry 2016 in Rostock ; Conference date: 08-06-2015 Through 11-06-2015",
url = "http://www.polymerphysik.uni-rostock.de/laehnwitzseminar/laehnwitz_2016/laehnwitz_con_2016.php",
}
RIS (suitable for import to EndNote) - Download
TY - CONF
T1 - Defect analysis in semicrystalline polymers using combined differential scanning calorimetry and X-ray line profile analysis
AU - Spieckermann, Florian
N1 - Conference code: 14th
PY - 2016/6
Y1 - 2016/6
M3 - Poster
T2 - Lähnwitz Seminar on Calorimetry 2016 in Rostock
Y2 - 8 June 2015 through 11 June 2015
ER -