Assessment of the stepped isothermal method for accelerated creep testing of high-density polyethylene

Publikationen: Beitrag in FachzeitschriftArtikelForschung(peer-reviewed)

Standard

Assessment of the stepped isothermal method for accelerated creep testing of high-density polyethylene. / Pilz, Gerald; Wurzer, Stefan; Morak, Matthias et al.
in: Mechanics of time-dependent materials, 2021.

Publikationen: Beitrag in FachzeitschriftArtikelForschung(peer-reviewed)

Bibtex - Download

@article{af69464d08fa4fa4b08c9ebcf5b5470f,
title = "Assessment of the stepped isothermal method for accelerated creep testing of high-density polyethylene",
keywords = "Accelerated creep testing, Creep properties, Dynamic mechanical analysis, High-density polyethylene, Stepped isothermal method",
author = "Gerald Pilz and Stefan Wurzer and Matthias Morak and Gerald Pinter",
note = "Publisher Copyright: {\textcopyright} 2021, The Author(s).",
year = "2021",
doi = "10.1007/s11043-021-09512-1",
language = "English",
journal = "Mechanics of time-dependent materials",
issn = "1385-2000",
publisher = "Springer Nature",

}

RIS (suitable for import to EndNote) - Download

TY - JOUR

T1 - Assessment of the stepped isothermal method for accelerated creep testing of high-density polyethylene

AU - Pilz, Gerald

AU - Wurzer, Stefan

AU - Morak, Matthias

AU - Pinter, Gerald

N1 - Publisher Copyright: © 2021, The Author(s).

PY - 2021

Y1 - 2021

KW - Accelerated creep testing

KW - Creep properties

KW - Dynamic mechanical analysis

KW - High-density polyethylene

KW - Stepped isothermal method

UR - http://www.scopus.com/inward/record.url?scp=85113590951&partnerID=8YFLogxK

U2 - 10.1007/s11043-021-09512-1

DO - 10.1007/s11043-021-09512-1

M3 - Article

AN - SCOPUS:85113590951

JO - Mechanics of time-dependent materials

JF - Mechanics of time-dependent materials

SN - 1385-2000

ER -