γ0.625pt′-size effect on the deformation microstructure and texture in a Ni-based superalloy using in-situ neutron diffraction

Publikationen: Beitrag in FachzeitschriftArtikelForschung(peer-reviewed)

Standard

γ0.625pt′-size effect on the deformation microstructure and texture in a Ni-based superalloy using in-situ neutron diffraction. / Yan, Zhiran; Srikakulapu, Kiranbabu; Gao, Yi et al.
in: Scripta materialia, Jahrgang 236.2023, Nr. November, 115665, 12.07.2023.

Publikationen: Beitrag in FachzeitschriftArtikelForschung(peer-reviewed)

APA

Yan, Z., Srikakulapu, K., Gao, Y., Qin, H., Rong, Y., Bi, Z., Xie, Q., An, K., Wang, Y., & Tan, Q. (2023). γ0.625pt′-size effect on the deformation microstructure and texture in a Ni-based superalloy using in-situ neutron diffraction. Scripta materialia, 236.2023(November), Artikel 115665. Vorzeitige Online-Publikation. https://doi.org/10.1016/j.scriptamat.2023.115665

Vancouver

Yan Z, Srikakulapu K, Gao Y, Qin H, Rong Y, Bi Z et al. γ0.625pt′-size effect on the deformation microstructure and texture in a Ni-based superalloy using in-situ neutron diffraction. Scripta materialia. 2023 Jul 12;236.2023(November):115665. Epub 2023 Jul 12. doi: 10.1016/j.scriptamat.2023.115665

Bibtex - Download

@article{5f8bd5ac3904485da559a1c7cdcf0037,
title = "γ0.625pt′-size effect on the deformation microstructure and texture in a Ni-based superalloy using in-situ neutron diffraction",
author = "Zhiran Yan and Kiranbabu Srikakulapu and Yi Gao and Hailong Qin and Yi Rong and Zhongnan Bi and Qingge Xie and Ke An and Yandong Wang and Qing Tan",
year = "2023",
month = jul,
day = "12",
doi = "10.1016/j.scriptamat.2023.115665",
language = "English",
volume = "236.2023",
journal = "Scripta materialia",
issn = "1359-6462",
publisher = "Acta Materialia Inc",
number = "November",

}

RIS (suitable for import to EndNote) - Download

TY - JOUR

T1 - γ0.625pt′-size effect on the deformation microstructure and texture in a Ni-based superalloy using in-situ neutron diffraction

AU - Yan, Zhiran

AU - Srikakulapu, Kiranbabu

AU - Gao, Yi

AU - Qin, Hailong

AU - Rong, Yi

AU - Bi, Zhongnan

AU - Xie, Qingge

AU - An, Ke

AU - Wang, Yandong

AU - Tan, Qing

PY - 2023/7/12

Y1 - 2023/7/12

U2 - 10.1016/j.scriptamat.2023.115665

DO - 10.1016/j.scriptamat.2023.115665

M3 - Article

VL - 236.2023

JO - Scripta materialia

JF - Scripta materialia

SN - 1359-6462

IS - November

M1 - 115665

ER -