Using lab-XRD to verify successful electrochemical hydrogen charging for in-situ nanoindentation

Research output: Contribution to conferencePosterResearchpeer-review

Standard

Using lab-XRD to verify successful electrochemical hydrogen charging for in-situ nanoindentation. / Jelinek, Anna; Zeiler, Stefan; Maier-Kiener, Verena.
2024. Poster session presented at EPRI Hydrogen Embrittlment Workshop, Oxford, United Kingdom.

Research output: Contribution to conferencePosterResearchpeer-review

Harvard

Jelinek, A, Zeiler, S & Maier-Kiener, V 2024, 'Using lab-XRD to verify successful electrochemical hydrogen charging for in-situ nanoindentation', EPRI Hydrogen Embrittlment Workshop, Oxford, United Kingdom, 23/06/24 - 26/06/24.

APA

Jelinek, A., Zeiler, S., & Maier-Kiener, V. (2024). Using lab-XRD to verify successful electrochemical hydrogen charging for in-situ nanoindentation. Poster session presented at EPRI Hydrogen Embrittlment Workshop, Oxford, United Kingdom.

Vancouver

Jelinek A, Zeiler S, Maier-Kiener V. Using lab-XRD to verify successful electrochemical hydrogen charging for in-situ nanoindentation. 2024. Poster session presented at EPRI Hydrogen Embrittlment Workshop, Oxford, United Kingdom.

Author

Bibtex - Download

@conference{8b0efc3e5a394c489e7f897f5232eb2b,
title = "Using lab-XRD to verify successful electrochemical hydrogen charging for in-situ nanoindentation",
author = "Anna Jelinek and Stefan Zeiler and Verena Maier-Kiener",
year = "2024",
language = "English",
note = "EPRI Hydrogen Embrittlment Workshop ; Conference date: 23-06-2024 Through 26-06-2024",

}

RIS (suitable for import to EndNote) - Download

TY - CONF

T1 - Using lab-XRD to verify successful electrochemical hydrogen charging for in-situ nanoindentation

AU - Jelinek, Anna

AU - Zeiler, Stefan

AU - Maier-Kiener, Verena

PY - 2024

Y1 - 2024

M3 - Poster

T2 - EPRI Hydrogen Embrittlment Workshop

Y2 - 23 June 2024 through 26 June 2024

ER -