Schadensanalyse an einer Kompaktierwalze aus Siliziumnitrid
Research output: Chapter in Book/Report/Conference proceeding › Conference contribution
Authors
Organisational units
External Organisational units
- Materials Division, National Physical Laboratory
Details
Original language | German |
---|---|
Title of host publication | Praktische Metallographie Sonderband |
Pages | 267-272 |
Volume | 52 |
Publication status | Published - 2018 |
Event | 15. Internationale Metallographie-Tagung - Montanuniversitaet Leoben, Leoben, Austria Duration: 19 Sept 2018 → 21 Sept 2018 |
Conference
Conference | 15. Internationale Metallographie-Tagung |
---|---|
Country/Territory | Austria |
City | Leoben |
Period | 19/09/18 → 21/09/18 |