Numerical simulation of the simultaneous precipitation of δ and γ′ phases in the Ni-base superalloy ATI Allvac®718 Plus™
Research output: Chapter in Book/Report/Conference proceeding › Conference contribution
Authors
Organisational units
External Organisational units
- Institute of Materials Science and Technology
- Institute for Materials Science and Welding
- Technische Universität Graz
- Böhler Schmiedetechnik GmbH and Co KG
Details
Original language | English |
---|---|
Title of host publication | 7th International Symposium on Superalloy 718 and Derivatives 2010 |
Pages | 569-578 |
Number of pages | 10 |
DOIs | |
Publication status | Published - 2010 |
Publication series
Name | 7th International Symposium on Superalloy 718 and Derivatives 2010 |
---|---|
Volume | 2 |