Nanoindentation of gas shales – analytical potential and limitations
Research output: Contribution to conference › Abstract › peer-review
Authors
Organisational units
External Organisational units
- GEOS4 GmbH
- China University of Geosciences, Beijing
- Erich Schmid Institute of Materials Science
Details
Original language | English |
---|---|
Publication status | Published - Sept 2020 |
Event | MSE Congress - Darmstadt, Germany Duration: 22 Sept 2020 → 25 Sept 2020 |
Conference
Conference | MSE Congress |
---|---|
Country/Territory | Germany |
City | Darmstadt |
Period | 22/09/20 → 25/09/20 |