Mechanical Variability of the S2 Layer in Wood Cell Walls by Nanoindentation
Research output: Chapter in Book/Report/Conference proceeding › Conference contribution
Authors
Organisational units
Details
Translated title of the contribution | Mechanical Variability of the S2 Layer in Wood Cell Walls by Nanoindentation |
---|---|
Original language | English |
Title of host publication | Proceedings of the 2nd International Symposium on Wood Machining |
Publisher | BOKU - Univ. of Natural Resources [u.a.] |
Pages | 45-51 |
Publication status | Published - 2004 |