Investigation of the slow crack growth behavior of static and cyclic loaded specimens of polyethylene by 2D and 3D optical fracture surface analysis

Research output: Contribution to journalArticleResearchpeer-review

Authors

Details

Translated title of the contributionInvestigation of the slow crack growth behavior of static and cyclic loaded specimens of polyethylene by 2D and 3D optical fracture surface analysis
Original languageEnglish
Pages (from-to)103-111
JournalMacromolecular Symposia
Volume311
DOIs
Publication statusPublished - 2012