Fractography of zirconia-specimens made using additive manufacturing (LCM) technology
Research output: Contribution to journal › Article › Research › peer-review
Authors
Organisational units
External Organisational units
- Lithoz GmbH
Details
Original language | English |
---|---|
Pages (from-to) | 4331-4338 |
Journal | Journal of the European Ceramic Society |
Volume | 37 |