FEM simulation of the effect of surface roughness on nanoindentation of thin films with a spherical indenter

Research output: Chapter in Book/Report/Conference proceedingConference contribution

Standard

FEM simulation of the effect of surface roughness on nanoindentation of thin films with a spherical indenter. / Walter, Claudia; Antretter, T.; Daniel, Rostislav et al.
34th International Conference on Metallurgical Coatings and Thin Films. 2007. p. 60-60.

Research output: Chapter in Book/Report/Conference proceedingConference contribution

Harvard

Walter, C, Antretter, T, Daniel, R & Mitterer, C 2007, FEM simulation of the effect of surface roughness on nanoindentation of thin films with a spherical indenter. in 34th International Conference on Metallurgical Coatings and Thin Films. pp. 60-60.

APA

Walter, C., Antretter, T., Daniel, R., & Mitterer, C. (2007). FEM simulation of the effect of surface roughness on nanoindentation of thin films with a spherical indenter. In 34th International Conference on Metallurgical Coatings and Thin Films (pp. 60-60)

Vancouver

Walter C, Antretter T, Daniel R, Mitterer C. FEM simulation of the effect of surface roughness on nanoindentation of thin films with a spherical indenter. In 34th International Conference on Metallurgical Coatings and Thin Films. 2007. p. 60-60

Author

Walter, Claudia ; Antretter, T. ; Daniel, Rostislav et al. / FEM simulation of the effect of surface roughness on nanoindentation of thin films with a spherical indenter. 34th International Conference on Metallurgical Coatings and Thin Films. 2007. pp. 60-60

Bibtex - Download

@inproceedings{e3f3ca6022284657bef9fcc931dd7bea,
title = "FEM simulation of the effect of surface roughness on nanoindentation of thin films with a spherical indenter",
author = "Claudia Walter and T. Antretter and Rostislav Daniel and Christian Mitterer",
year = "2007",
language = "English",
pages = "60--60",
booktitle = "34th International Conference on Metallurgical Coatings and Thin Films",

}

RIS (suitable for import to EndNote) - Download

TY - GEN

T1 - FEM simulation of the effect of surface roughness on nanoindentation of thin films with a spherical indenter

AU - Walter, Claudia

AU - Antretter, T.

AU - Daniel, Rostislav

AU - Mitterer, Christian

PY - 2007

Y1 - 2007

M3 - Conference contribution

SP - 60

EP - 60

BT - 34th International Conference on Metallurgical Coatings and Thin Films

ER -