Exploring the mechanical character of molybdenum grain boundaries via nanoindentation and three-point-bending
Research output: Contribution to conference › Poster › Research
Authors
Organisational units
External Organisational units
- PLANSEE SE
- Erich Schmid Institute of Materials Science
Details
Original language | English |
---|---|
Publication status | Published - 2019 |
Event | ECI Nanomechanical Testing in Materials Research and Development - Torremolinos, Spain Duration: 29 Sept 2019 → 4 Oct 2019 |
Conference
Conference | ECI Nanomechanical Testing in Materials Research and Development |
---|---|
Country/Territory | Spain |
City | Torremolinos |
Period | 29/09/19 → 4/10/19 |