Correlation of local mechanical properties and chemical compositin in a C-containing TiAl alloy studied by nanoindentation and atom probe tomography
Research output: Contribution to conference › Poster › Research
Authors
Organisational units
External Organisational units
- Erich Schmid Institute of Materials Science
Details
Original language | English |
---|---|
Publication status | Published - 2017 |
Event | Summer School "Eperimental Nano-und Micromechanics" - Düsseldorf, Austria Duration: 11 Sept 2017 → 15 Sept 2017 |
Workshop
Workshop | Summer School "Eperimental Nano-und Micromechanics" |
---|---|
Country/Territory | Austria |
City | Düsseldorf |
Period | 11/09/17 → 15/09/17 |