Advanced creep testing of refractories providing new insight into material behaviour
Research output: Contribution to journal › Article › Research › peer-review
Standard
Advanced creep testing of refractories providing new insight into material behaviour. / Jin, Shengli; Harmuth, Harald; Gruber, Dietmar et al.
In: Refractories worldforum, Vol. 10, No. 2, 2018, p. 63-67.
In: Refractories worldforum, Vol. 10, No. 2, 2018, p. 63-67.
Research output: Contribution to journal › Article › Research › peer-review
Harvard
Jin, S, Harmuth, H, Gruber, D, Schachner, S, Meunier, P & Techer, R 2018, 'Advanced creep testing of refractories providing new insight into material behaviour', Refractories worldforum, vol. 10, no. 2, pp. 63-67. <http://refractories-worldforum.com/php/article_pdf.php?article_id=100633&hash=3468335bd5>
APA
Vancouver
Jin S, Harmuth H, Gruber D, Schachner S, Meunier P, Techer R. Advanced creep testing of refractories providing new insight into material behaviour. Refractories worldforum. 2018;10(2):63-67.
Author
Bibtex - Download
@article{ba2fd0179a1f4f6b85f7f39c50864d51,
title = "Advanced creep testing of refractories providing new insight into material behaviour",
author = "Shengli Jin and Harald Harmuth and Dietmar Gruber and Stefan Schachner and Pierre Meunier and Romain Techer",
year = "2018",
language = "English",
volume = "10",
pages = "63--67",
journal = "Refractories worldforum",
issn = "1868-2405",
number = "2",
}
RIS (suitable for import to EndNote) - Download
TY - JOUR
T1 - Advanced creep testing of refractories providing new insight into material behaviour
AU - Jin, Shengli
AU - Harmuth, Harald
AU - Gruber, Dietmar
AU - Schachner, Stefan
AU - Meunier, Pierre
AU - Techer, Romain
PY - 2018
Y1 - 2018
UR - https://www.refractories-worldforum.com/order/all-articles.html?article_id=100633
M3 - Article
VL - 10
SP - 63
EP - 67
JO - Refractories worldforum
JF - Refractories worldforum
SN - 1868-2405
IS - 2
ER -