Actual versus apparent within cell wall variability of nanoindentation results from wood cell walls related to cellulose microfibril angle
Research output: Contribution to journal › Article › Research › peer-review
Standard
Actual versus apparent within cell wall variability of nanoindentation results from wood cell walls related to cellulose microfibril angle. / Konnerth, J.; Gierlinger, N.; Keckes, Jozef et al.
In: Journal of materials science, Vol. 44, 2009, p. 4399-4406.
In: Journal of materials science, Vol. 44, 2009, p. 4399-4406.
Research output: Contribution to journal › Article › Research › peer-review
Harvard
Konnerth, J, Gierlinger, N, Keckes, J & Gindl, W 2009, 'Actual versus apparent within cell wall variability of nanoindentation results from wood cell walls related to cellulose microfibril angle', Journal of materials science, vol. 44, pp. 4399-4406.
APA
Konnerth, J., Gierlinger, N., Keckes, J., & Gindl, W. (2009). Actual versus apparent within cell wall variability of nanoindentation results from wood cell walls related to cellulose microfibril angle. Journal of materials science, 44, 4399-4406.
Vancouver
Konnerth J, Gierlinger N, Keckes J, Gindl W. Actual versus apparent within cell wall variability of nanoindentation results from wood cell walls related to cellulose microfibril angle. Journal of materials science. 2009;44:4399-4406.
Author
Bibtex - Download
@article{2117fa3c3be04d24ac5336a5429b3037,
title = "Actual versus apparent within cell wall variability of nanoindentation results from wood cell walls related to cellulose microfibril angle",
author = "J. Konnerth and N. Gierlinger and Jozef Keckes and W. Gindl",
year = "2009",
language = "English",
volume = "44",
pages = "4399--4406",
journal = "Journal of materials science",
issn = "0022-2461",
publisher = "Springer",
}
RIS (suitable for import to EndNote) - Download
TY - JOUR
T1 - Actual versus apparent within cell wall variability of nanoindentation results from wood cell walls related to cellulose microfibril angle
AU - Konnerth, J.
AU - Gierlinger, N.
AU - Keckes, Jozef
AU - Gindl, W.
PY - 2009
Y1 - 2009
M3 - Article
VL - 44
SP - 4399
EP - 4406
JO - Journal of materials science
JF - Journal of materials science
SN - 0022-2461
ER -