Investigations of thermally activated deformation processes in W-Re alloys by high temperature nanoindentation up to 800 °C

Activity: Talk or presentation Oral presentation

Participants

Date

24 Apr 2019

Johann Kappacher - Speaker

Alexander Leitner - contributor

Helmut Clemens - contributor

Verena Maier-Kiener - contributor

24 Apr 2019

Event (Seminar)

Title65. Metallkunde‐Kolloquium
Period24/04/1926/04/19
CityLech am Arlberg
Country/TerritoryAustria
Degree of recognitionInternational event