δ-phase characterization of superalloy Allvac 718 Plus™
Publikationen: Beitrag in Buch/Bericht/Konferenzband › Beitrag in Konferenzband
Standard
TMS2008 - 137th Annual Meeting and Exhibition Supplemental Proceedings: Materials Processing and Properties. 2008. S. 63-68 (TMS Annual Meeting; Band 2).
Publikationen: Beitrag in Buch/Bericht/Konferenzband › Beitrag in Konferenzband
Harvard
APA
Vancouver
Author
Bibtex - Download
}
RIS (suitable for import to EndNote) - Download
TY - GEN
T1 - δ-phase characterization of superalloy Allvac 718 Plus™
AU - Sommitsch, Christof
AU - Stotter, Christoph
AU - Leitner, Harald
AU - Mitsche, Stefan
AU - Letofsky-Papst, Ilse
AU - Stockinger, Martin
PY - 2008
Y1 - 2008
KW - Allvac 718Plus™
KW - Delta-phase
KW - Nickel-base superalloy
UR - http://www.scopus.com/inward/record.url?scp=52249117670&partnerID=8YFLogxK
M3 - Conference contribution
AN - SCOPUS:52249117670
SN - 9780873397179
T3 - TMS Annual Meeting
SP - 63
EP - 68
BT - TMS2008 - 137th Annual Meeting and Exhibition Supplemental Proceedings
T2 - TMS 2008 Annual Meeting Supplemental: Materials Processing and Properties
Y2 - 9 March 2008 through 13 March 2008
ER -