Fast differential scanning calorimetry to mimic additive manufacturing processing: specific heat capacity analysis of aluminium alloys
Publikationen: Beitrag in Fachzeitschrift › Artikel › Forschung › (peer-reviewed)
Standard
in: Journal of Thermal Analysis and Calorimetry, Jahrgang ???, Nr. ??? Stand: 5. Jänner 2023, 2022.
Publikationen: Beitrag in Fachzeitschrift › Artikel › Forschung › (peer-reviewed)
Harvard
APA
Vancouver
Author
Bibtex - Download
}
RIS (suitable for import to EndNote) - Download
TY - JOUR
T1 - Fast differential scanning calorimetry to mimic additive manufacturing processing
T2 - specific heat capacity analysis of aluminium alloys
AU - Quick, Cameron
AU - Dumitraschkewitz, Phillip
AU - Schawe, Jürgen E.K.
AU - Pogatscher, Stefan
N1 - Publisher Copyright: © 2022, The Author(s).
PY - 2022
Y1 - 2022
KW - Additive manufacturing (AM)
KW - Aluminium alloys
KW - Fast differential scanning calorimetry (FDSC)
KW - Precipitation
KW - Specific heat capacity
UR - http://www.scopus.com/inward/record.url?scp=85143516358&partnerID=8YFLogxK
U2 - 10.1007/s10973-022-11824-4
DO - 10.1007/s10973-022-11824-4
M3 - Article
AN - SCOPUS:85143516358
VL - ???
JO - Journal of Thermal Analysis and Calorimetry
JF - Journal of Thermal Analysis and Calorimetry
SN - 1388-6150
IS - ??? Stand: 5. Jänner 2023
ER -