Elastic Modulus of Cr2AlC Thin Films Probed by Nanoindentation
Publikationen: Konferenzbeitrag › Poster › Forschung › (peer-reviewed)
Standard
Elastic Modulus of Cr2AlC Thin Films Probed by Nanoindentation. / Sigumonrong, D.P.; Schneider, J.M.; Music, D. et al.
2007. Postersitzung präsentiert bei Hysitron Europe Workshop 2007, Ismaning, Deutschland.
2007. Postersitzung präsentiert bei Hysitron Europe Workshop 2007, Ismaning, Deutschland.
Publikationen: Konferenzbeitrag › Poster › Forschung › (peer-reviewed)
Harvard
Sigumonrong, DP, Schneider, JM, Music, D, Walter, C, Emmerlich, J, Iskandar, R, Mayer, J, Korte, S & Clegg, WJ 2007, 'Elastic Modulus of Cr2AlC Thin Films Probed by Nanoindentation', Hysitron Europe Workshop 2007, Ismaning, Deutschland, 18/10/07 - 19/10/07.
APA
Sigumonrong, D. P., Schneider, J. M., Music, D., Walter, C., Emmerlich, J., Iskandar, R., Mayer, J., Korte, S., & Clegg, W. J. (2007). Elastic Modulus of Cr2AlC Thin Films Probed by Nanoindentation. Postersitzung präsentiert bei Hysitron Europe Workshop 2007, Ismaning, Deutschland.
Vancouver
Sigumonrong DP, Schneider JM, Music D, Walter C, Emmerlich J, Iskandar R et al.. Elastic Modulus of Cr2AlC Thin Films Probed by Nanoindentation. 2007. Postersitzung präsentiert bei Hysitron Europe Workshop 2007, Ismaning, Deutschland.
Author
Bibtex - Download
@conference{92a408dbd6b9442cb448c7aa1a35bcc8,
title = "Elastic Modulus of Cr2AlC Thin Films Probed by Nanoindentation",
author = "D.P. Sigumonrong and J.M. Schneider and D. Music and Claudia Walter and J. Emmerlich and R. Iskandar and J. Mayer and S. Korte and W.J. Clegg",
year = "2007",
language = "English",
note = "Hysitron Europe Workshop 2007 ; Conference date: 18-10-2007 Through 19-10-2007",
}
RIS (suitable for import to EndNote) - Download
TY - CONF
T1 - Elastic Modulus of Cr2AlC Thin Films Probed by Nanoindentation
AU - Sigumonrong, D.P.
AU - Schneider, J.M.
AU - Music, D.
AU - Walter, Claudia
AU - Emmerlich, J.
AU - Iskandar, R.
AU - Mayer, J.
AU - Korte, S.
AU - Clegg, W.J.
PY - 2007
Y1 - 2007
M3 - Poster
T2 - Hysitron Europe Workshop 2007
Y2 - 18 October 2007 through 19 October 2007
ER -