Characterization of a Biocompatible Co-Cr-W Alloy by means of Correlative Microscopy and Nanoindentation Experiments
Publikationen: Konferenzbeitrag › Poster › Forschung
Standard
Characterization of a Biocompatible Co-Cr-W Alloy by means of Correlative Microscopy and Nanoindentation Experiments. / Weißensteiner, Irmgard; Voigt, Patrick; Clemens, Helmut et al.
2017. Postersitzung präsentiert bei TMS 2017, San Diego, CA, USA / Vereinigte Staaten.
2017. Postersitzung präsentiert bei TMS 2017, San Diego, CA, USA / Vereinigte Staaten.
Publikationen: Konferenzbeitrag › Poster › Forschung
Harvard
Weißensteiner, I, Voigt, P, Clemens, H & Maier-Kiener, V 2017, 'Characterization of a Biocompatible Co-Cr-W Alloy by means of Correlative Microscopy and Nanoindentation Experiments', TMS 2017, San Diego, CA, USA / Vereinigte Staaten, 26/02/17 - 2/03/17.
APA
Weißensteiner, I., Voigt, P., Clemens, H., & Maier-Kiener, V. (2017). Characterization of a Biocompatible Co-Cr-W Alloy by means of Correlative Microscopy and Nanoindentation Experiments. Postersitzung präsentiert bei TMS 2017, San Diego, CA, USA / Vereinigte Staaten.
Vancouver
Weißensteiner I, Voigt P, Clemens H, Maier-Kiener V. Characterization of a Biocompatible Co-Cr-W Alloy by means of Correlative Microscopy and Nanoindentation Experiments. 2017. Postersitzung präsentiert bei TMS 2017, San Diego, CA, USA / Vereinigte Staaten.
Author
Bibtex - Download
@conference{31fed121fab641158060833d427d7a67,
title = "Characterization of a Biocompatible Co-Cr-W Alloy by means of Correlative Microscopy and Nanoindentation Experiments",
author = "Irmgard Wei{\ss}ensteiner and Patrick Voigt and Helmut Clemens and Verena Maier-Kiener",
year = "2017",
language = "English",
note = "TMS 2017 ; Conference date: 26-02-2017 Through 02-03-2017",
}
RIS (suitable for import to EndNote) - Download
TY - CONF
T1 - Characterization of a Biocompatible Co-Cr-W Alloy by means of Correlative Microscopy and Nanoindentation Experiments
AU - Weißensteiner, Irmgard
AU - Voigt, Patrick
AU - Clemens, Helmut
AU - Maier-Kiener, Verena
PY - 2017
Y1 - 2017
M3 - Poster
T2 - TMS 2017
Y2 - 26 February 2017 through 2 March 2017
ER -